Froth flotation of Azara barite ore was carried out using a mixture of available raw materials, the burnt empty palm (Eleasis guineesis) bunch solution, and analytical grade palmitic acid as collector, sodium silicate as depressant. Optimum recovery was obtained at collector concentration of 0.01 moles litre-1. Energy Dispersive X-ray spectrophotometric analysis of the feed ore and concentrate showed an increase from 75.4 % to 91.1 % BaSO4, respectively. The variation of flotation parameters show that between pH range of 4 and 10 and equilibration time of 10 minutes, barite recovery increased. Analysis of the processed palm bunch showed that its major chemical component is K2O (52.1%) which generates KOH on hydrolysis. The investigation reveals that palmitic acid and palm bunch product is a good collector for barite.


में अनुक्रमित

  • कैस
  • गूगल ज्ञानी
  • जे गेट खोलो
  • चीन राष्ट्रीय ज्ञान अवसंरचना (सीएनकेआई)
  • उद्धरण कारक
  • ब्रह्मांड IF
  • इलेक्ट्रॉनिक जर्नल्स लाइब्रेरी
  • रिसर्च जर्नल इंडेक्सिंग की निर्देशिका (डीआरजेआई)
  • गुप्त खोज इंजन लैब्स
  • आईसीएमजेई

और देखें

Flyer